direct buy china factory cobalt-based electrode/cobalt base alloy welding rod aws a5.13 ECoCr-A 3.15mm

Unit Price: 35~75 USD
Min. Order: 80 Kilogram

Product Description

Product Description

 

direct buy china factory cobalt-based electrode/cobalt base alloy welding rod aws a5.13 ECoCr-A  3.15mm

GB/T984
EDCoCr-A-03
AWS A5.13: ECoCr-A

Introduction:

D802 is a kind of hardfacing electrode for titanium calcium type,and with CoCrMo casting alloy core,coating by dipping into the legal system,suitable for DC reverse

Application:

direct buy china factory cobalt-based electrode/cobalt base alloy welding rod aws a5.13 ECoCr-A 3.15mm

Used for surfacing welding on occasions requiring excellent wear-resistance, corrosion-resistance enough under 650℃,such as the surfacing welding of high temperature and pressure valves,hot shearing knives etc.Also used for surfacing welding on workpieces under the conditions withstood impact and alternated cooling and heating.

Chemical Composition of Deposited Metal (%) 

Chemical Composition

C

Cr

Mn 

Si

W

Requirement

1.00~1.70

26.00~32.00

≤2.00

≤2.00

7.00~10.00

 

Deposited Metal Hardness: HRC≥40 

Diameters/Reference Current (DC+)

direct buy china factory cobalt-based electrode/cobalt base alloy welding rod aws a5.13 ECoCr-A 3.15mm

Electrode Diameter (mm)

3.2

4.0

5.0

Welding Current (A)

120-160 

140-190

150-210

Notes on Usages:

1.The electrodes must be baked under 200℃ for an hour before welding.

2.As far as possible with short arc welding, and welding work to maintain the vertical.

3.According to the size of the work and the type of the base material should be 300~600 preheating.

4.After the welding, it should be in 600 ~ 700 tempering after 1 hour in slowly cooled or will work immediately placed in dry and hot sandbox or Barilla slow cooling, to avoid cracks.

5.The surfacing layer must be rough grinding, if found defects, according to the above steps to weld repair and slow cooling.

application

direct buy china factory cobalt-based electrode/cobalt base alloy welding rod aws a5.13 ECoCr-A 3.15mm

package and delivery

Package details:

5kg/inner box,   4boxes/carton=20kg ,50cartons=1 ton/pallet;

 

Delivery:

Time: Normally ready goods within 8 to 25 days.

Term: CIF CNF FOB EXW

direct buy china factory cobalt-based electrode/cobalt base alloy welding rod aws a5.13 ECoCr-A 3.15mmdirect buy china factory cobalt-based electrode/cobalt base alloy welding rod aws a5.13 ECoCr-A 3.15mm 

FAQ

Q: are your trading company or manufacturer?

A:we are factory

Q:how long is your delivery time:

A:Generally it's 7-15 days if the goods are in stock,or it's 15-20days if goods are not in stock,it depends on quantity.

Q:Do you provide free sample?it's free or extra?

A:yes,we offer free sample,but don't pay the cost of freight.

Q:what is your payment term?

A:payment<=1000usd,100% in advance.payment>1000usd ,30%TT in advance,balance before shippment.
If you have another question, pls feel free to contact us as below:

contact us

      direct buy china factory cobalt-based electrode/cobalt base alloy welding rod aws a5.13 ECoCr-A 3.15mm       

Contact us if you need more details on Cobalt Base Alloy Rod. We are ready to answer your questions on packaging, logistics, certification or any other aspects about Cobalt-based Electrode、Welding Rod Ecocr-a. If these products fail to match your need, please contact us and we would like to provide relevant information.

Product Categories : welding electrodes/rods > cobalt base rod